Purifying?agent?for?molten?zinc?in?HDG
Name:
Purifying?agent?for?molten?zinc?in?HDG
  • Model:
  • Uses:
  •  
Details

In the light of the high iron and impurity contents in molten zinc, poor fluidness and particles and fold on workpiece often occurred in hot galvanizing plants, our company has organized the famous specialists and scientific and technological personnel in many disciplines at home developed XY-XG-3 type purifying agent for molten zinc, a high and new technical product. It has effectively solved the difficult problem and filled in the gap in this field at home. Through testing and using, the agent reached the anticipated results and is well received by customers. At present the product is applying for a patent. 
Notice
Do well pretreatment work, do not carry the harmful impurity into zinc pot, galvanizing agent needs the acid and iron eliminating, and it would be best if rinsing water for pretreatment could be fluid.
Because of the high volatility of the agent, No.2 operation should be quickly performed.
In order to avoid the splashing of molten zinc causing danger, operators should be well dressed in labor protection articles. Operation with caution and safety first.
Purifying Treatment Method of Molten Zinc:
Keep furnace temperature at 450℃-470℃.
Place dry thermal insulation bricks (with strong water absorption) into box with holes, quickly pour the purifying agent to them, insert the box into molten zinc and move it back and forth until boiling ends, and take out the box with holes.
Eliminate suspended substances on the surface of molten zinc; scatter ammonium chloride (1-1.5 kg/ m2) to further eliminate impurity on the surface.
Repeat the abovementioned steps three or four times.
Add the alloy, which is 0.5% of molten zinc, in uniform distribution way. After all the melting, repeat the abovementioned step once. (If there are excessive aluminum or other alloys in original molten zinc, the step-by-step method can be used)
The temperature is controlled at 430℃-440℃ and the standing time is 6-12 h (time is as long as possible).
When small workpiece is tested (the temperature is at 430℃ and dipping time is not changed), the surface and coating thickness is measured. If the coating is thick, the alloy, which is 0.1 % of molten zinc, can be added. 
The zinc and the alloy can be added at one time until the alloy content in molten zinc reaches 1.5%.
After alloying is completed, the working temperature of molten zinc should be controlled at 440℃±5℃ and the lifting speed of traveling crane at 1.5 m / min.
 

 

返回頂部 電話
主站蜘蛛池模板: 久久精品国产亚洲一区二区| 制服丝袜日韩欧美| 91av手机在线观看| 好看的国产精品| 中文字幕日韩哦哦哦| 日韩在线视频一区二区三区| 亚洲国产成人片在线观看| 深夜影院一级毛片| 免费网站看av片| 美国成人免费视频| 成人一a毛片免费视频| 久久婷婷五月综合97色| 欧美videosgratis蛇交| 亚洲日本va午夜中文字幕一区| 玉蒲团之天下第一| 内射一区二区精品视频在线观看| 色一情一乱一伦色一情一乱一伦| 国产又色又爽又黄的在线观看| 婷婷综合五月天| 婷婷无套内射影院| 中文字幕一精品亚洲无线一区 | 三级网站免费观看| 成人做受视频试看60秒| 久久偷看各类wc女厕嘘嘘| 最新国产福利在线观看| 亚洲免费观看在线视频| 欧美精品v国产精品v日韩精品 | 天堂资源在线中文| zzzzzzz中国美女| 快点cao我要被cao烂了| 三个黑人上我一个经过| 成全高清视频免费观看| 中文字幕无码av激情不卡| 日本一区二区三区日本免费 | 日韩美女视频一区| 亚洲AV日韩精品久久久久久 | 国产一级淫片免费播放| 视频一区二区在线观看| 国产亚洲欧美在在线人成| 青青青在线观看视频免费播放| 国产又粗又大又爽又黄|